Facing bricksBrick H

Technische informatie

Kleur omschrijving
The colour of the body is brown and it has strong nuances ranging from brown to brown-purple with chalk white accents
Afmeting (L x B x H)
ca. 224x73x54 mm (LxBxH)
Aantal / m² met een traditionele voeg
65 (12 mm)
Aantal / m² met een dunne voeg
73 (6 mm)
Afmeting 2
ca. 215x100x65 mm (LxBxH) - On demand > 2000 m²

reportage Brick H

Creativity with facing bricks defines look of office building

Creativity with facing bricks defines look of office building

Brick has been and still is the most durable and timeless material

CAW Oost-Vlaanderen is in the process of constructing an office building with primary care facilities and 16 short-stay units on the site of a former brewery in the heart of Sint-Gillis-bij-Dendermonde. 

Referenties

Zoek volgens gemeente





Referentie lijst Brick H
Postcode Stad Straat Metselverband Voeg Voegkleur Raam Dakbedekking Opmerkingen
9800 Deinze St-Hubert-Straat 57 Random bond 6 mm
9031 Drongen Luchterenstraat 29 Random bond 6 mm
9970 Kaprijke Bloemstraat Random bond 6 mm
3360 Lovenjoel Weterbeekstraat Random bond 6 mm White
9090 Melle Jan De Lichte Random bond 6 mm
8470 Moere Zandhilweg Random bond 6 mm
4140 Sprimont-Lincé Rue Abeé de Marteau 10 Random bond 6 mm
9240 Zele Klein Ruiveld Random bond 6 mm
9840 Zevergem Pont Noord 101 Random bond 6 mm
Print alle

Verwerkingstips

Preparation of the construction site

Quality brickwork starts with the proper storage of the materials. Provide a firm level base so that bricks are not in contact with rain and/or dirt.  
As clay is a natural material, successive production runs of the same kind of bricks may present colour variations and size tolerances.
The following precautions will help minimizing this:
  • Always order the full amount of bricks required for a specific site. In this way, the entire order can be made during one production run.
  • Try to have the full order supplied at one time. If this creates several deliveries, always mix a number of packs from the previous delivery with a number of packs from the new delivery. This procedure is especially recommended in case of re-order or for an additional order.
  • Take bricks diagonally across the pack.
  • Draw and use bricks from at least five different packs.
  • For setting out, use bricks from the delivery made to the site in question. Do not exclusively use the theoretical dimensions of the brick, or samples previously supplied, or different production run from that intended for the site.
  • As soon as the bricks arrive on site, check delivery tickets and certificates against the specification and order. Also check that there are no visible inconsistencies with the order.
  • Do not lay bricks in freezing weather or protect the ‘fresh’ masonry with insulating mats in order to avoid frost damage to the mortar.
  • In the case of prolonged dry hot weather, lightly dampen the newly laid brickwork to stop the mortar drying and curing too quickly.
  • Do not lay bricks in precipitation in order to prevent mortar from running on the wall.

Avoid Efflorescence

Brickwork is sometimes marred by white bloom. This efflorescence is usually caused because bricklaying is done under unfavourable weather conditions. The necessary protective measures are often not implemented due to a tight schedule and fast building pace. In very wet conditions, water in soluble substances can result in efflorescence on the surface. In spring as well as autumn, after a wet period (when the brickwork has dried again), soluble substances can rise to the surface as a result of moisture transport. After evaporation of the water, a white bloom is left behind. (Source: Efflorescence on brickwork – Heidelberg Cement Group)
 
Efflorescence on brickwork is always likely to occur. There is no brick - or combination of a certain brick with a specific mortar - that is absolutely efflorescence-free. By taking a few simple precautions, the risk of efflorescence can be reduced.
  • During and after laying, protect the newly built brickwork for a height of at least 60 cm - but ensure there is airspace between the brick face and the waterproof covering.